INCOLOY 800
X10NiCrAITi32.20
1.4876
Z10NC32.21
UNS 08800
N08800
NA16
Base Element Fe(Iron)
Element | Min | Max |
---|---|---|
Al(Aluminium) | 0.15% | 0.6% |
C(Carbon) | 0.1% | |
Cr(Chromium) | 19% | 23% |
Fe(Iron) | 39.5% | |
Ni(Nickel) | 30% | 35% |
Ti(Titanium) | 0.15% | 0.6% |
Heat Treatment; Produced using annealing procedures that result in optimum creep and rupture properties. If subjected to hot or cold forming, re-annealing may be necessary to restore creep and rupture strength or to prevent cold-formed parts from recrystallising during high temperature service. Re-annealing must be done at 1150 degs C.
Bolting
Various uses in the Aerospace, Petrochemical, Chemical. Offshore engineering, Marine, Thermal-processing, Electrical and Electronics industries. Used for its high heat performance and corrosion resisting metals.
Disclaimer:
Information is given for illustrative purposes only. Tachart accepts no responsibility for the accuracy of the data contained within or the use of the data by any other party.
This page is protected by copyright but may be freely distributed but not reproduced without permission.