Chemistry

Element Min Max
C (Carbon) 0.015% (maximum)
Cr (Chromium) 20% 22.5%
Co (Cobalt) 2.5%
Cu (Copper) 0.5%
Fe (Iron) 2% 6%
Mn (Manganese) 0.5%
Mo (Molybdenum) 12.5% 14.5%
Si (Silicon) 0.08%
W (Tungsten) 3% 3%
V (Vanadium) 0.35%
Ultimate Tensile Strength (UTS) 690 MPa
0.2% Proof Stress 310 MPa
Elongation 45%

Uses Of HASTELLOY C22

Bolting
Used for its high corrosion resistance in hydrofluoric acid and bleach environments.