Chemistry

Stainless Steel
Base Element Fe (Iron)

Element Min Max
C (carbon) 0.14 0.23%
Cr (Chromium) 15.5 1.7%
Mn(Manganese) 1%
Ni(Nickel) 1.5 2.5%
P (Phosphorus) 0.045%
S (Sulphur) 0.03%
Si (Silicon) 1%

Mechanical Property,Statistic,(Max/Min)
Ultimate Tensile Strength (UTS),850,1000 MPa
Yield Strength, 680 MPa,
0.2% Proof Stress, 635 MPa,
Elongation,11%,
Gauge Length,5.65vSo
Hardness (Brinell),248,302 HB
Izod Impact = Room Temp,0.365,KJ/m^2(minimum)

Uses

Typically used in nuts and bolting, Marine Systems, Pumps and propellers.