HASTELLOY C22

Désolé, cet article est seulement disponible en Anglais Américain. Pour le confort de l’utilisateur, le contenu est affiché ci-dessous dans une autre langue. Vous pouvez cliquer le lien pour changer de langue active.

Alias

HASTELLOY C22
NiCr21Mo14W
2.4602
UNS N6022

Chemistry

Element Min Max
C (Carbon) 0.015% (maximum)
Cr (Chromium) 20% 22.5%
Co (Cobalt) 2.5%
Cu (Copper) 0.5%
Fe (Iron) 2% 6%
Mn (Manganese) 0.5%
Mo (Molybdenum) 12.5% 14.5%
Si (Silicon) 0.08%
W (Tungsten) 3% 3%
V (Vanadium) 0.35%
Ultimate Tensile Strength (UTS) 690 MPa
0.2% Proof Stress 310 MPa
Elongation 45%

Uses Of HASTELLOY C22

Bolting
Used for its high corrosion resistance in hydrofluoric acid and bleach environments.

Disclaimer:
Information is given for illustrative purposes only. Tachart accepts no responsibility for the accuracy of the data contained within or the use of the data by any other party.
This page is protected by copyright but may be freely distributed but not reproduced without permission.

error: Content is Copyright Tachart Bolt & Nut Manufacturing !!